How do I eliminate “checking” or "alligatoring" (the fracturing the board surface) at the decurl station?
When decurling 0.028” thick (500 gsm) coated recycled board, the surface of the sheet gets cracked. What can I do?
From time to time, we have to sheet poorly wound rolls with baggy edges. How do you compensate for this roll defect?
Should I run material down the center of the machine or off an edge?
When I run multiple webs of light weight material, it sometimes wrinkles prior to cutting. How do I avoid that?